Hardness(shore A) | 69 | 67 | 66 | 65 | 64 | 63 |
Tensile strength(Mpa) | 11.5 | 13.1 | 12.1 | 13.9 | 10.9 | 13.6 |
Elongation(%) | 270 | 300 | 305 | 350 | 290 | 380 |
Compression set(%) | +27 | +28 | +28 | +29 | +28 | +29 |
Ozone-resistance(50pphm, 40°C, 3day) | No Crack | No Crack | No Crack | No Crack | No Crack | No Crack |
Low temperature resistance(TR-10) | −47.9 | −44.6 | −48.9 | −50.5 | −51.9 | −52.6 |
Heat resistance (120°C, 70hr) | Hardness change(%) | +8 | +9 | +9 | +10 | +10 | +11 |
Tensile strength change(%) | +15.7 | +18.3 | +33.1 | +14.4 | +46.8 | +33.8 |
Elongation change(%) | −40.7 | −33.3 | −31.1 | −35.7 | −24.1 | −36.8 |
Oil resistance (ASTM IRM 901, 120°C, 70hr) | Hardness change(%) | +2 | +3 | +4 | +5 | +4 | +5 |
Tensile strength change(%) | +23.5 | +13.0 | +28.1 | +0.4 | +21.1 | +17.6 |
Volume change(%) | −2.9 | −4.7 | −5.6 | −9.5 | −7.5 | −7.9 |
Oil resistance (ASTM IRM 903, 120°C, 70hr) | Hardness change(%) | −8 | −7 | −7 | −6 | −6 | −5 |
Tensile strength change(%) | +5.2 | −9.2 | +1.7 | −5.0 | −5.7 | −8.6 |
Volume change(%) | +18.2 | +18.0 | +16.7 | +15.5 | +13.4 | +14.2 |