Table 6. Degradation Temperatures of B-200 Synthesized at NCO Index 200 with Dabco K-15, Dabco TMR-30, and Toyocat RX-5

The used catalyst 1st degradation 2nd degradation
Tini (K) Tinf (K) Tterm (K) Tini (K) Tinf (K) Tterm (K)
Dabco K-15 444.1 549.9 576.2 713.5 802.8 873.0
Dabco TMR-30 517.7 603.0 658.6 742.6 849.0 919.6
Toyocat RX-5 504.2 580.5 608.8 711.8 802.6 878.2