Table 7. Degradation Temperatures of B-300 Synthesized at NCO Index 300 with Dabco K-15, Dabco TMR-30, and Toyocat RX-5

The used catalyst 1st degradation 2nd degradation
Tini (K) Tinf (K) Tterm (K) Tini (K) Tinf (K) Tterm (K)
Dabco K-15 480.2 561.9 581.4 699.8 803.3 862.8
Dabco TMR-30 510.6 598.9 648.3 719.6 814.1 876.5
Toyocat RX-5 516.2 589.8 655.2 711.8 809.5 885.1