Table 3. Dynamic Viscoelastic Characteristics Data of Silica–SBR Compounds according to Extend Oil Content

Tg (°C) Tan δ at Tg E' at –30°C (MPa) E'' at 0°C (MPa) Tan δ at 60°C
O40 −41.915 1.019 40.96 2.798 0.1107
O20 −41.664 0.864 74.26 4.542 0.1179
O15 −39.383 0.830 92.31 5.787 0.1163
O10 −38.990 0.861 72.48 3.604 0.1096