Table 3. Dynamic Viscoelastic Properties of the Silica-SBR Compounds According to Types of Cellulose Based Dispersants
Compounds
WN
WC
WCMC
WNC
T
g
(°C)
−35.38
−41.85
−39.37
−39.10
Tanδ at T
g
0.768
0.935
0.867
1.070
E’ at –30°C (MPa)
116.4
54.85
91.04
40.89
E’’ at 0°C (MPa)
6.739
3.156
5.400
1.462
Tanδ at 60°C
0.078
0.058
0.076
0.051